MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 Brick Grease NLGI No. 6+
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Brick Grease is a hard, amber-colored, smooth-textured, lithium-based grease made in block or brick form. Brick Grease provides a high melting point block grease with good heat resistance. It is designed for the lubrication of open heavy-duty bearings equipped with open well top feed grease collars, such as: Kiln, trunnion and support wall bearings; Ball, tube, rod and comped mill bearings; Paper machine dryer section; Cement mills, jack shaft bearings, crushers, rolling mills, rubber compounding mills, etc.; Kiln dryers; Dehydrators

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 8181Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 450 - 550 SUS450 - 550 SUSBase Oil Property
Saybolt Viscosity at 210°F 55 - 65 SUS55 - 65 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 105 cSt105 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 10.5 cSt10.5 cStBase Oil
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 45 - 6545 - 65
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 129 °C265 °F
Minimum Service Temperature, Air -12.2 °C10.0 °F
Dropping Point 196 °C385 °F
 
Descriptive Properties
ColorMedium Amber
Soap Type (Thickener)Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON199 / 75236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.