Description: Notch-resistant, condensation crosslinking silicone filling compound particularly for casting polyester resin Key Features - Good flowing behavior
- Very good elastic properties
- Outstanding stability to polyester resins
- Suitable for block moulds and skin moulds with strong undercuts
Cured Product: Standard climate DIN 50 014 - 23/50-2. Vulcanizate tested after 7 days at room temperatureInformation provided by CHT Group |