MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Polyethylene (PE)

Material Notes: Product Description: Exxelor VA 1803 polymer resin is a high flow, amorphous ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in outstanding thermal and oxidative stability leading to enhanced weaterability. Moreover, its amorphous nature exhibits impact resistance at very low temperatures in blends with engineering polymers such as polyamide. This grade is designed to:
  • Modify the impact characteristics of the full range of polyamides for temperatures as low as -40°C (a function of the modifier treat level in the blend).
  • Offer the best balance between stiffness and low temperature performance in polyamide blends.
  • Modify the impact characteristics of other engineering thermoplastic and technical polymers (with or without glass fibers, fillers, etc.)
  • Achieve compatibility between polyolefins and more polar polymers that are capable of interacting with maleic anhydride.

Key Features: Performance enhancements in polyamide blends:

  • Outstanding notched Izod impact resistance at room temperature.
  • Consistent and very high notched Izod impact resistance down to -40°C
  • Improved flexibility
  • Reduced moisture sensitivity and improved dimensional stability allowing the production of molded parts with different wall thickness
  • Improved assembly of freshly molded parts
  • Increased impact resistance of glass-reinforced compositions.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/ccExxonMobil Method
Melt Flow 3.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 22 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
Collected Volatile Condensable Material <= 0.15 %AM-S 350.03
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -59.0 °CDSC
 
Optical PropertiesOriginal ValueComments
Yellow Index <= 20 %ASTM E313-96
 
Descriptive Properties
Maleic anhydride graft levelhigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXXELOR™ VA 1840 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber

PEXB510 / 37815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.