MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass  (discontinued **)
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/cc
Thickness 1000 microns
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
Transformation Temperature, Tg 418 °C
Softening Point 441 °CDilatometric
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.60
Transmission, Visible 15.7 %Photopic, Source 2100 K
 5.0 %
@Wavelength 580 nm
 32 %
@Wavelength 480 nm
 50 %
@Wavelength 520 nm
UV Transmittance 2.0 %
@Wavelength 380 nm
 9.0 %
@Wavelength 400 nm
 9.0 %
@Wavelength 420 nm
 
Descriptive Properties
Chromaticity, CIE 19760.1u', Source 2100 K
 0.55v', Source 2100 K
NVIS Radiance4.4E-12NR(b), MIL-STD-3009@0.1 fL Luminance, Source 2100 K
 6.5E-11NR(a), MIL-STD-3009@0.1 fL Luminance, Source 2100 K
Tolerance Radius0.01r', Source 2100 K

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMOSCI005 / 137188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.