MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mechanical breaking point due to the good bond between the carbon fiber and nickel. Used in thermoplastic compounds for EMI shielding. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
Thickness 0.250 micronsNi Coating Thickness
Fiber Count 7200 dtex
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 34000 kg(f)/cm²
Elongation at Break 1.5 %
Tensile Modulus 2.30e+6 kg(f)/cm²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Toho Tenax Besfight® MC Type II (3000 Filament) Nickel Coated Carbon Fiber
Toho Tenax Besfight® MC Type II (6000 Filament) Nickel Coated Carbon Fiber
Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber

ETOHO02 / 6103

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.