MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Superwool® Boards and Shapes Plus PM Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: AES Fiber Class. Superwool boards are processed from a slurry consisting of Superwool bulk fiber and organic binders. Each board has cut edges for controlled squareness and trueness. Boards may be ordered with both surfaces machined smooth to a close thickness tolerance. Superwool is a low bio-persistent fiber, manufactured from pure raw materials and processed to offer excellent performance in high-temperature applications. Superwool offers an alternative to traditional solutions due to its high refractoriness and excellent non-wetting characteristics with molten aluminum. Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (e.g. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying. Superwool is ideally suited to individual applications and is available in a wide range of thicknesses and densities. The maximum continuous use temperature depends on the application.

Applications:

  • Molten aluminum contact
  • Furnace, kiln, and oven hot face linings
  • Flue and chimney linings
  • Insulation as backup to:- firebrick- insulating firebrick- refractory castables- rammed shapes
  • Appliance and heat processing insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.240 - 0.270 g/cc0.00867 - 0.00975 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00140 - 0.00170 GPa
@Temperature 982 °C
0.203 - 0.247 ksi
@Temperature 1800 °F
fired
Compressive Strength 0.100 - 0.170 MPa14.5 - 24.7 psiat 5% deformation
 0.160 - 0.280 MPa23.2 - 40.6 psiat 10% deformation
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
 0.0900 W/m-K
@Temperature 538 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 0.140 W/m-K
@Temperature 816 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
Melting Point 1275 °C2327 °F
Maximum Service Temperature, Air 1000 °C1830 °FContinuous Use
Shrinkage 1.0 %
@Temperature 816 °C,
Time 86400 sec
1.0 %
@Temperature 1500 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
CaO+MgO 27 %27 %
Loss on Ignition(%) 2.0 - 4.0 %2.0 - 4.0 %
Other 1.0 %1.0 %
SiO2 67 %67 %
 
Descriptive Properties
Classification Temperature (°C)1100
Colorbeige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF7092 / 203390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.