MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Bada BADAMID® A70 GF50 natural Nylon 66, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Heat-stabilized polyamide 66 injection molding grade with 50% glass fiber reinforcement for mechanically and thermally stressed articles

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccISO 1183
Moisture Absorption 1.40 %50% r.h.; ISO 62
Water Absorption at Saturation 4.3 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 225 MPa5 mm/min; ISO 527-1/2
Elongation at Break 2.5 %5 mm/min; ISO 527-1/2
Tensile Modulus 16700 MPa1 mm/min; ISO 527-1/2
Flexural Strength 315 MPaISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC-62631-3-1
Surface Resistance 1.00e+12 ohmIEC-62631-3-2
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC-62631-2-1
Dissipation Factor 0.015
@Frequency 1e+6 Hz
IEC-62631-2-1
Comparative Tracking Index 550 VIEC-60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 57.0 µm/m-°CISO 11359-2
Melting Point 262 °C10 K/min; ISO 3146
Maximum Service Temperature, Air 230 °Csome hours; EC-60216
 110 °C
@Time 7.20e+7 sec
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/2
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm
Glow Wire Ignition Temperature 675 °C
@Thickness 0.750 mm
IEC-60695-2-13
 675 °C
@Thickness 1.60 mm
IEC-60695-2-13
Glow Wire Flammability Index 650 °C
@Thickness 0.750 mm
IEC-60695-2-12
 650 °C
@Thickness 1.60 mm
IEC-60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBADA024 / 286857

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.