MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Embrace™ Encore Renew-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: The world's leading shrink film just got better with the introduction of Eastman Embrace™ Encore Renew-50 to the Eastman Embrace™ family of resins. Eastman Embrace™ Encore Renew-50 was designed to produce shrinkable films that are compatible with the PET recycling process while still offering superior shrinkable film performance. Shrinkable film performance is modified by making changes to the extruders manufacturing process. Eastman Embrace™ Encore Renew-50 emulates all visually satisfying attributes expected from the current Eastman Embrace™ such as high gloss and clarity. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED. The GREENGUARD INDOOR AIR QUALITY CERTIFIED®; Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.spot.ul.com . Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Decorative laminates-cabinetry
  • Decorative laminates-wood
  • Home, garden & automotive packaging
  • Labels non food contact
  • Multi-layer film non food contact
  • Shrink film non food contact
Key Attributes
  • Customizable shrink curve
  • Eye-catching 360° graphic capability
  • Greater than 60% ultimate shrinkage
  • High toughness
  • Recognized by the Association for Plastics
  • Recycling to be compatible with the PET recycling process when used in combination with washable inks
  • Shrinks to fit contour bottles
  • Sparkling clarity and high gloss
  • Super-high print definition

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccASTM D1505
Viscosity Measurement 0.700Inherent, film, EMN-A-AC-G-V-1
 0.700Inherent, pellet, EMN-A-AC-G-V-1
Thickness 50.0 microns
Surface Tension 2.80 dynes/cmHarmonic Mean, Polar
 41.7 dynes/cmHarmonic Mean, Dispersive
 43.2 - 45.8 dynes/cmHarmonic Mean, Total
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 390 %ASTM D882
Film Elongation at Break, TD 588 %ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 206 °CASTM D1525
Glass Transition Temp, Tg 75.0 °CASTM D1525
Shrinkage >= 60.0 %
@Temperature 95.0 °C
Ultimate
 
Optical PropertiesOriginal ValueComments
Haze 0.500 %99.5% Clarity; ASTM D1003
 0.800 %ASTM D1003
Gloss 143 %60°; ASTM D2457
 
Descriptive Properties
Agglomeration with rPET flake (%)0.27APR PET-CG-02 target <1%
Color-0.05a*, ASTM D2244
 0.47b*, ASTM D2244
 2.45b*, Pellet, ASTM D2244
 -2.47a*, Pellet, ASTM D2244
 58.5L*, Pellet, ASTM D2244
 95.8L*, ASTM D2244
Ring Crush278 psiM.D.; Tappi T822
Shrink Force10 MPa80°C, ISO 14616

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4136 / 323759

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.