MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum A357.0-T61, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium A357.0-T61; UNS A13570; AAA357.0-T61; AlA357.0-T61
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.67 g/cc0.0965 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 85 - 11585 - 115AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 126126Estimated from Brinell Hardness.
Hardness, Rockwell A 4141Estimated from Brinell Hardness.
Hardness, Rockwell B 6363Estimated from Brinell Hardness.
Hardness, Vickers 113113Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 310 MPa>= 45000 psiAA
Tensile Strength, Yield >= 248 MPa
@Strain 0.2 %
>= 36000 psi
@Strain 0.2 %
AA
Elongation at Break >= 3.0 %>= 3.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 72.4 GPa10500 ksiCompressive modulus in is typically about 2% higher for Al alloys
Poissons Ratio 0.330.33Calculated Value
Machinability 50 %50 %0-100 Scale (100=best)
Shear Modulus 26.8 GPa3890 ksi
Shear Strength 187 MPa27100 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 ohm-cm0.00000440 ohm-cmAA; Typical 39% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  21.4 µm/m-°C
@Temperature 20.0 - 100 °C
11.9 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical
 23.2 µm/m-°C
@Temperature 20.0 - 300 °C
12.9 µin/in-°F
@Temperature 68.0 - 572 °F
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°F
Thermal Conductivity 151 W/m-K1040 BTU-in/hr-ft²-°FAA; Typical at 25°C
Melting Point 557.2 - 612.8 °C1035 - 1135 °FAA; Typical
Solidus 557.2 °C1035 °FAA; Typical
Liquidus 612.8 °C1135 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Solution Temperature 540.6 °C1005 °Fhold at temperature for 8 hr; hot water quench
Aging Temperature 171 °C340 °Fhold at temperature 3 to 5 hrs
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.7 - 93 %90.7 - 93 %As remainder
Beryllium, Be 0.04 - 0.07 %0.04 - 0.07 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 0.20 %<= 0.20 %
Magnesium, Mg 0.40 - 0.70 %0.40 - 0.70 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 6.5 - 7.5 %6.5 - 7.5 %
Titanium, Ti 0.04 - 0.20 %0.04 - 0.20 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A357.0-T62, Cast
Aluminum 357.0-T6, Permanent Mold Cast
Aluminum A357.2 Composition Spec
Aluminum 357.0-F Casting Alloy
Aluminum A356.0-T61, Permanent Mold Cast

MAC3570AT6 / 9947

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.