MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ineos Nova S-2200 Medium Impact Compact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Medium impact easy flowing polystyrene, designed for injection molding applications with short cycle times and for complicated technical parts. The product has a high stiffness and an excellent thermal stability under heat. For certain applications a non lubricated type has to be preferred.

All mechanical properties measured under standard conditions 50% RH and 23°C.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccDIN 53479
Water Absorption <= 0.10 %DIN 53495
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
DIN 5375/ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 120 MPaDIN 53456
Tensile Strength, Ultimate 40.0 MPaDIN 53455
Elongation at Break 20 %DIN 53455
Modulus of Elasticity 2.40 GPaDIN 53457
Flexural Yield Strength 50.0 MPaDIN 53452
Izod Impact, Notched (ISO) 3.00 kJ/m²Low Temp; DIN 53453
 4.50 kJ/m²DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) 40.0 kJ/m²DIN 53453
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Thermal Conductivity 0.160 W/m-KDIN 52612
Vicat Softening Point 96.0 °CDIN 53460

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSI 825E Polystyrene
Total 965E Polystyrene
Total 680 Polystyrene
Ineos Nova 4501 Medium Impact Polystyrene
Ineos Nova 4211 Medium Impact Polystyrene

PNOVA082 / 54983

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.