MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Versalis Impressio® ABS B 10 3D Printing Filament Grade ABS Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Impressio® ABS B10 is an easily process able ABS with good mechanical and thermal properties. The product has been optimized for the production of filaments dedicated to 3D printing (FDM), and its properties makes it compatible with most of the commercial 3D printers. The processing technology used to produce Impressio® ABS B10 makes it one of the cleanest grades on the market (low organic volatile content).

Applications: Impressio® ABS B10 has been designed to produce 1.75 and 2.85mm filaments used into 3D printers for the production of prototypes or final goods.

Information provided by Versalis.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
0.30 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Thickness 1750 - 2850 microns68.9 - 112 milFor filament production.
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
25 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ISO 2039/2
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ISO 527
Elongation at Yield 2.8 %2.8 %50 mm/min; ISO 527
Tensile Modulus 2.35 GPa341 ksi1 mm/min; ISO 527
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
6.66 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmDry; IEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
Dry; IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inDry; IEC 60243
Dissipation Factor 0.015
@Frequency 1000 Hz
0.015
@Frequency 1000 Hz
Dry; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FASTM C 177
Vicat Softening Point 98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
50°C/h; ISO 306/B 50
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Test 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
IEC 60695-2-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 240 °C410 - 464 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9899 / 265635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.