MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aperam AS11 Cold Rolled Strip Thermostatic bimetal (large temperature range)
Categories: Metal; Ferrous Metal

Material Notes: Aperam bimetals “AS… series” find very wide application regarding its high constant deflection, and its good transformation performance.

International standards: DIN-1715 , ASTM-B388

Typical Chemical composition:
Passive Component: Fe Ni36
Intermediate layer: Nickel and Copper
Active Component: Fe Ni20 Mn6

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000102 - 0.0000117 ohm-cm0.0000102 - 0.0000117 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 µm/m-°C
@Temperature -20.0 - 200 °C
8.33 µin/in-°F
@Temperature -4.00 - 392 °F
Maximum Service Temperature, Air 400 °C752 °F
 
Descriptive Properties
Spec thermal curvature26.68-28.91[10e-06/K°]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
BASF Ultraform® N2320 006 POM
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Nabaltec ACTILOX® B60 AS1 AlO(OH) Boehmite
Nabaltec ACTILOX® 200 AS1 AlO(OH) Boehmite

NPERA061 / 194850

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.