MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

United Soft Plastics Unisoft Adhesion AD-65A-NT-4-10 Nylon Adhesion Grade Polyurethane-based Thermoplastic Elastomer (TPE-U)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: This compound is used for overmolding onto a variety of polyamide substrates. It is available worldwide.

Features:

  • Easily Colorable
  • Heat Stabilized
  • Good Resilience
  • High Elongation
  • Excellent Chemical Resistance
  • High Strength

Information provided by United Soft Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Linear Mold Shrinkage 0.012 - 0.018 cm/cm0.012 - 0.018 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565
Tensile Strength 13.2 MPa1910 psi
Elongation at Break 500 %500 %
100% Modulus 4.07 MPa
@Strain 100 %
590 psi
@Strain 100 %
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 185 °C340 - 365 °F
Middle Barrel Temperature 185 - 199 °C365 - 390 °F
Front Barrel Temperature 199 - 216 °C390 - 420 °F
Nozzle Temperature 204 - 224 °C400 - 435 °F
Drying Temperature 79.4 °C
@Time 7200 - 10800 sec
175 °F
@Time 2.00 - 3.00 hour
 
Descriptive Properties
BondingPA6, PA6-GF, PA6,6, PA6,6-GF
Colorsnatural, black, and precolored
ProcessingInjection Molding
Relative FlowHIGH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSOF9821 / 243324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.