MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Phillips 66 Wet Gas Compressor Oil ISO Grade 220
Categories: Fluid; Lubricant

Material Notes: Wet Gas Compressor Oil is a high-quality lubricant developed for the lubrication of oil-flooded rotary compressors in natural gas service. It also is recommended for cylinder lubrication of reciprocating compressors in natural gas service. It is specially formulated to minimize the effects of gas dilution and oil absorption and to resist wash-off in compressors handling “wet” gas (natural gas containing liquid hydrocarbons and/or water). Wet Gas Compressor Oil is specially formulated to provide excellent service and protection in gas compression service. It has excellent oxidation resistance and thermal stability at high temperatures to help minimize deposit formation and provide long service life. It is compounded with an oiliness additive that provides good metal-wetting ability to help resist lubricant wash-off in the presence of wet gas. It protects against rust, corrosion and wear, and is resistant to excessive foaming that can interfere with proper lubrication. Wet Gas Compressor Oil is particularly recommended for use in applications where the gas outlet temperature is well above the condensation point of the gas.

Applications:

  • Oil-flooded rotary screw, rotary lobe and rotary vane compressors handling wet natural gas
  • Industrial reciprocating compressors pumping wet natural gas
  • Reciprocating compressors commonly found in remote gas gathering stations
Features/Benefits:
  • Excellent oxidation resistance and thermal stability
  • Resists lubricant “wash-off”
  • Formulated to minimize the effects of gas dilution and oil absorption
  • Good wear protection
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.889 g/cc
Density 7.40 lb/gal
Viscosity Measurement 94Index
Saybolt Viscosity at 100°F 1154 SUS
Saybolt Viscosity at 210°F 94.6 SUS
Kinematic Viscosity at 40°C (104°F) 218 cSt
Kinematic Viscosity at 100°C (212°F) 18.5 cSt
Oxidative Stability 4000 hourASTM D943-04a
ASTM Color 2.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.14[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.400 mmScar Diameter; ASTM D2266
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °C
Flash Point 285 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility15 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5045 / 198298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.