MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Bicor® 120 SLP OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminating side.

Availability: Latin America, North America and South America

Key Features:

  • Excellent ink adhesion and bond strength in adhesive, PVdC adhesive, and extrusion laminations
  • Non-migratory slip system for consistent COF
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crisps and Snacks
  • Fresh Produce
Uses:
  • HFFS Flexible Packaging
  • Pouches – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 4.30 g/m²/day
@Temperature 38.0 °C
0.277 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 30.5 microns1.20 milNominal; ExxonMobil Method
Coating Weight 27.4 g/m²17.1 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.200.20slip modified; ExxonMobil Method
Film Tensile Strength at Break, MD 124 MPa18000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 241 MPa35000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.0 %
@Temperature 135 °C
4.0 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 4.5 %
@Temperature 135 °C
4.5 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ExxonMobil Method
Gloss 88 %88 %45°, Untreated Surface; ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.83 receding COS thetaPrint Surface
Yield25500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXB432 / 37737

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.