MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NuSil CV10-2568 Silicone, Two Part Adhesive and Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Two Part Adhesive and Sealant

Comments: Fast Cure, Low Density

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.760 g/cc
Viscosity 80000 cPB
 125000 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength at Break 1.62 MPa
Elongation at Break 170 %
Shear Strength 1.20 MPaLap, Primed with CF1 -135
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 860 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 245 µm/m-°C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
Working Life 3.00 hour
 
Descriptive Properties
ColorRed
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
NuSil R31-2186 Silicone Two Part Sealing & Adhesive
NuSil R-2145 Silicone Two Part Sealing & Adhesive
NuSil CV-2568 Silicone, Two Part Adhesive and Sealant
NuSil CV-2566 Silicone, Two Part Adhesive and Sealant

PNUSIL176 / 141900

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.