MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Pure Element

Material Notes: Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides corrosion resistance in neutral to moderately reducing environments. In the annealed condition, either alloy possesses the approximate strength of mild steel. As-rolled material is sometimes furnished to provide higher strength levels. Uses include containers and piping in caustic soda and food processing plants.

This nickel alloy is readily fabricated by standard fabricating practices. The material are covered by a variety of specification and are assigned maximum allowable stresses in the ASME Boiler and Pressure Vessel Code. This alloy provides high thermal and electrical conductivity in comparison to nickel base alloys, stainless and low alloy steels. AL 201 Alloy is ferromagnetic.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4068, ASTM B-162; ASME SB-162; AMS 5533
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4545Typical Annealed
Tensile Strength, Ultimate 403 MPa58500 psiTypical Annealed
Tensile Strength, Yield 103 MPa
@Strain 0.2 %
14900 psi
@Strain 0.2 %
Typical; Annealed
Elongation at Break 50 %50 %typical in 2"; Annealed
Modulus of Elasticity 207 GPa30000 ksi
Poissons Ratio 0.310.31
Shear Modulus 81.0 GPa11700 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000850 ohm-cm0.00000850 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.3 µm/m-°C
@Temperature 27.0 - 93.0 °C
7.39 µin/in-°F
@Temperature 80.6 - 199 °F
 14.4 µm/m-°C
@Temperature 27.0 - 316 °C
8.00 µin/in-°F
@Temperature 80.6 - 601 °F
Specific Heat Capacity 0.456 J/g-°C0.109 BTU/lb-°F
Thermal Conductivity 67.1 W/m-K
@Temperature 100 °C
466 BTU-in/hr-ft²-°F
@Temperature 212 °F
Maximum Service Temperature, Air 427 °C801 °FCreep is a concern above this temp
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Copper, Cu 0.020 %0.020 %
Iron, Fe 0.050 %0.050 %
Manganese, Mn 0.020 %0.020 %
Nickel, Ni 99.9 %99.9 %as balance; includes Co
Silicon, Si 0.050 %0.050 %
Sulfur, S 0.0020 %0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson C 201 Commercially Pure Nickel
Special Metals Nickel 201
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 20% Cold Work
Special Metals Nickel 200

NLN201 / 18009

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.