MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

EOS NickelAlloy IN718 DMSL on EOS M 300-4; 40 µm
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Nickel Alloy

Material Notes: EOS NickelAlloy IN718 is a precipitation hardening nickel-chromium alloy that is characterized by having good tensile, fatigue, creep and rupture strength at temperatures up to 700 °C (1,290 °F).

Main Characteristics:

  • Parts are easily precipitation hardened
  • Parts can be machined, spark-eroded, welded, micro shot-peened, polished and coated
  • Chemical composition corresponding to UNS N07718, AMS 5662, AMS 5664, W.Nr 2.4668, DIN NiCr19Fe19NbMo3
Typical Applications:
  • Gas turbine components
  • Instrumentation parts
  • Power industry parts
  • Process industry parts
Heat treatment procedure in accordance with AMS 5662

Information provided by EOS GmbH (Electro Optical Systems).

Key Words: UNS N07718
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity <= 0.050 %<= 0.050 %
Thickness 40.0 microns1.57 mil
Pore Size <= 100 microns<= 3.94 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 957 MPa139000 psiVertical, as manufactured
 1092 MPa158400 psiHorizontal, as manufactured
 1370 MPa199000 psiVertical, heat treated
 1531 MPa222100 psiHorizontal, heat treated
Tensile Strength, Yield 634 MPa92000 psiVertical, as manufactured
 796 MPa115000 psiHorizontal, as manufactured
 1141 MPa165500 psiVertical, heat treated
 1267 MPa183800 psiHorizontal, heat treated
Elongation at Break 15 %15 %Horizontal, heat treated
 20 %20 %Vertical, heat treated
 27 %27 %Horizontal, as manufactured
 36 %36 %Vertical, as manufactured
 
Descriptive Properties
Volume rateup to 4 x 4.2 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS932 / 280592

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.