Pro-fax SD242 nucleated impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers an excellent stiffness/impact balance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax SD242. Availability: North America Application: Interior Automotive Applications; TWIM Food Containers Market: Automotive; Rigid Packaging Processing Method: Compounding; Injection Molding Attribute: General Purpose; Nucleated Information provided by LyondellBasell. |