MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU HOLLOW BELT-1038 Hollow belt
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • Can join belts quickly and reliably with a connector
  • Excellent abrasion resistance and flexibility
  • Great to oils, fuels and oxygen
  • Great belt for light duty conveying and transfer
Application: Hollow belt can use for transmission purposes of newspaper, textile machines, packaging machines, printing presses, food machinery, ceramic processing plants, cannery conveying equipment, wood-working machine, floor and roof tiles and industrial and paper industry machines. Widely used in the facilities line, the glaze, polishing lines and transmission line. Hollow belt can be jointed quickly and reliably by fitting connector.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 83 - 8783 - 87ASTM D2240
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D412
Elongation at Break 520 %520 %ASTM D412
Tear Strength 74.5 kN/m425 pliASTM D412
Abrasion 4949[mg]; ASTM D746
Compression Set 12 %12 %25% Deformation
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FSolenoid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU379 / 306109

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.