MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Hostalen ACP 9255 B HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hostalen ACP 9255 B is a high density polyethylene resin which possesses an outstanding combination of stiffness and impact performance. Hostalen ACP 9255 B can be processed on blown film lines at high output rates with excellent bubble stability, very low gel levels and homogeneous appearance which converters and end-users require for high quality thin and thick film production. Hostalen ACP 9255 B can enable the production of films with a very broad conversion window, good lay flat properties and excellent roll configuration. Typical applications are lamination and release films, artificial paper, labels, bags and heavy duty packaging.

Availability: Asia-Pacific

Application: Bags & Pouches; Food Packaging Film; Heavy Duty Packaging; Lamination Film; Products for Use in Property Modification

Market: Flexible Packaging

Processing Method: Blown Film

Attribute: Antioxidant; Good Drawdown; Good Toughness; High Rigidity; Low Gel

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ISO 1183-1
Melt Flow  0.400 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.400 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 12.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 450 %450 %ISO 527-1, -3
Film Elongation at Break, TD 470 %470 %ISO 527-1, -3
Tensile Modulus 1.35 GPa196 ksiISO 527-1, -2
Elmendorf Tear Strength MD 20.0 g20.0 gISO 6383-2
Elmendorf Tear Strength TD 80.0 g80.0 gISO 6383-2
Dart Drop Test 250 g0.551 lbASTM D1709
Film Tensile Strength at Break, MD 65.0 MPa9430 psiISO 527-1, -3
Film Tensile Strength at Break, TD 55.0 MPa7980 psiISO 527-1, -3
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FPeak; ISO 11357-3
Vicat Softening Point 76.0 °C169 °FISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9620 / 324555

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.