MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F650 Bismaleimide Resin
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: HexPly® F650 is a bismaleimide resin that cures via an additional/free radical mechanism resulting in a cross-linked thermoset system with no condensation by-products. HexPly® F650 was developed by Hexcel to overcome existing limitations for use on complex structures and ducting in advanced military aircraft, helicopters, and many other high temperature applications. HexPly® F650 simplifies fabrications and delivers a more cost-effective end product.

Advantages: Viscous, homogenous; Simple, adjustable, reaction kinetics; No resin advancement at room temperature; Simple processing and impregnation; High glass temperature relative to post cure, Dimensionally stable at greater than 500°F (260°C); High laminate mechanical strengths and strains; modest cost; Non-micro cracking for woven laminates

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/cc
Moisture Absorption at Equilibrium 4.3 %
 
Mechanical PropertiesOriginal ValueComments
Fracture Toughness 0.460 MPa-m½
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µm/m-°C
Maximum Service Temperature, Air >= 260 °Cdimensionally stable
Glass Transition Temp, Tg >= 316 °C
Flame Spread Index 10BMI/F650; ASTM E162
 15 - 20Epoxy/Typical; ASTM E162
Smoke Density <= 25µ g/m3; BMI/F650; ASTM E-662
 >= 300µ g/m3; Epoxy/Typical; ASTM E-662
 
Processing PropertiesOriginal ValueComments
Gel Time 5.00 - 8.00 min
@Temperature 177 °C
 
Descriptive Properties
Toxicity (smoke) (ppm), ASTM 662>25Epoxy/Typical
 5/10/2009BMI/F650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg Neat Resin
Solvay CORFIL® 5250-4 Potting Compound
Hexcel® HexPly® F652 Bismaleimide Resin
HOS-Technik Homide 250 Bismaleimide Resin
Solvay HTM® 552 Bismaleimide Resin

PHEXC001 / 98471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.