MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inov Chem INOVOL F4700 Polyether Polyols
Categories: Polymer

Material Notes: Introduction: This series of polyether polyol is suitable for producing flexile foam like sponge and packing material. And some of them are used for producing high resilience foam system.

Applications: BHT free, no amine, typical high activity polyether. Could be mixed with polymer polyether polyols, widely used for manicuring cold curing high resilience foam such as the seat cushion of automobile, motorcycle and bicycle. Also used for car steering wheel.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 5.0 - 7.0
Viscosity 900 - 1500 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.080[mgKOH/g]
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.050 %
 
Descriptive Properties
Color=30APHA
Degree of unsaturation=0.08 mol/Kg
K+=5 mg/Kg
OH value32-36 mgKOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM307 / 312836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.