MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Description

Polyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness.

NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.942 g/ccASTM D792
ESCR 100% Igepal® >= 500 hourASTM D1693
Melt Index of Compound 6.0 g/10 min2.16/190; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2600 psi2"/min; ASTM D638
Elongation at Break 400 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 105000 psiASTM D790
Impact Test 42.0 ft-lb
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM impact
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °CASTM D648
 
Descriptive Properties
UV StabilizationUV-8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ICO Polymers ICORENE™ 150-1501 HDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1498 HDPE Rotational Molding Resin
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
ICO Polymers ICORENE™ 150-1049 HDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1497 HDPE Rotational Molding Resin

PASHU063 / 25027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.