MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M FM532 White Polyester Label Products
Categories: Polymer; Adhesive

Material Notes: 3M™ White Polyester Label Products FM53R2, FM532 and FM782 are durable, high performance materials that utilize 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adhesive exhibits high initial tack, yet resists edge bleed and cold flow.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milFacestock
 78.7 microns3.10 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.701 kN/m4.00 pli180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °F
Minimum Service Temperature, Air 5.00 °C41.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 13.0 °C>= 55.4 °FApplication
 <= 49.0 °C<= 120 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive TypeP1110 Perm 26
Appearance50# SC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33814 / 168561

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.