MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Xenia Materials XECARB® 40-C30-M31 PC, 30% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes:

Information provided by Xenia Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inSim. ISO 294-4
Linear Mold Shrinkage, Transverse 0.0015 cm/cm0.0015 in/inSim. ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psi5 mm/min; ISO 527
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527
Tensile Modulus 19.0 GPa2760 ksi1 mm/min; ISO 527
Flexural Strength 230 MPa33400 psi2 mm/min; ISO 178
Flexural Modulus 16.2 GPa2350 ksi2 mm/min; ISO 178
Flexural Strain at Break 2.0 %2.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
50 % RH; ISO 180
Izod Impact, Unnotched (ISO)  30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 30.0 kJ/m²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
50 % RH; ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.050 ohm-cm0.050 ohm-cmIEC 60093
Surface Resistance 500 ohm500 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F120°C/h; ISO 75
Deflection Temperature at 8.0 MPa 125 °C257 °F120°C/h; ISO 75
Vicat Softening Point 155 °C
@Load 1.02 kg
311 °F
@Load 2.25 lb
120°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 295 °C554 - 563 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 80.0 - 100 °C176 - 212 °Fdesiccant dryer
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourdesiccant dryer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PXENIA954 / 268530

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.