MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro DESMODUR® TGF223 + BAYTEC® RG202, 35 A Polyurethane, TDI- PPG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccBAYTEC® RG202
 1.02 g/cc1.02 g/cc
 1.04 g/cc1.04 g/ccDESMODUR® TGF223
Viscosity 85 cP85 cPBAYTEC® RG202
 5000 cP5000 cPDESMODUR® TGF223
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535DIN 53505
 34
@Temperature 80.0 °C
34
@Temperature 176 °F
DIN 53505
 37
@Temperature -5.00 °C
37
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 6.00 MPa870 psiDIN 53504
Tensile Stress at Strain 0.300 MPa
@Strain 10 %
43.5 psi
@Strain 10 %
DIN 53504
Elongation at Break 1000 %1000 %DIN 53504
100% Modulus 1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
DIN 53504
200% Modulus 1.60 MPa
@Strain 200 %
232 psi
@Strain 200 %
DIN 53504
300% Modulus 2.10 MPa
@Strain 300 %
305 psi
@Strain 300 %
DIN 53504
Resilience 6868[%]; DIN 53512
Tear Strength 10.0 kN/m57.1 pliwith nick; ISO 34-1
 22.0 kN/m126 pliwithout nick; ISO 34-1
Abrasion 230230[mm3]; ISO 4649
Compression Set 23 %
@Temperature 70.0 °C,
Time 79200 sec
23 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FDESMODUR® TGF223
 25.0 °C77.0 °FBAYTEC® RG202
Mold Temperature 20.0 °C68.0 °F
Pot Life 17.0 min17.0 min
 
Descriptive Properties
AppearanceliquidDESMODUR® TGF223
 liquidBAYTEC® RG202
Content100Parts by weight of prepolymer
 2.1-2.5%NCO, DESMODUR® TGF223
 63Parts by weight of BAYTEC® RG202

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0625 / 202408

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.