MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Michelman® Michem® 4075B Water-based polyurethane dispersion
Categories: Fluid; Polymer

Material Notes: Michem® Dispersion Urethanes are water-based polyurethane dispersions that can enhance toughness, scratch resistance, water resistance and flexibility of coatings. Michem Dispersion Urethanes are useful for industrial wood, concrete, and metal substrates. Usage: Provides excellent abrasion resistance, water resistance, and high flexibility for floor coatings, parquet lacquers, and industrial coatings. This dispersion is compatible with most common additives, pigments, and pigment preparations and can be combined with other emulsions. Due to the variety of products in the market, compatibility and storage stability have to be tested from case to case. Polyurethane thickeners are highly recommended but most commercial thickeners can be used. Due to the dispersion, it is not mandatory to add coalescing agents. For application properties of the final product, it might be helpful to add co-solvents like glycol ethers.

Applications (properties imparted): Concrete (abrasion resistance, block resistance, flexibility, water resistance), OEM Applied Wood Protection (abrasion resistance, block resistance, flexibility, water resistance), On-Site Applied Wood Protection (abrasion resistance, block resistance, flexibility, water resistance), Textiles (abrasion resistance, flexibility, water resistance).

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 39 - 41 %Non-Volatiles
pH 7.0 - 8.0
Brookfield Viscosity 20 - 200 cPSpindle #2. 20 RPM.
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite liquid
Solids TypePolyurethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHE9861 / 287456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.