MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HB Fuller Advantra® PHC-9254 Hot melt adhesive
Categories: Polymer; Adhesive

Material Notes: Type of Product: Hot Melt Adhesive

Product Benefits: A superior, wide range grade case & carton hot melt adhesive with great performance at both low and high temperatures. An outstanding troubleshooting grade. It provides a unique combination of benefits, including a very fast speed of set, robust adhesion, extended open time, high hot tack, unequaled thermal stability, light color, low odor, a smoke-free environment, low density, increased mileage, and clean machining.

Typical Applications: Hot Fill to Blast Freezer, Cases, Cartons, Trays, Bliss Box, Hot and cold environments, High springback containers.

Suitable Substrates: Uncoated to moderately coated Corrugated, Clay Coated, SBS, SUS and similar materials

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Viscosity  785 cP
@Temperature 191 °C
785 cP
@Temperature 375 °F
 1015 - 1285 cP
@Temperature 177 °C
1015 - 1285 cP
@Temperature 350 °F
 1655 cP
@Temperature 163 °C
1655 cP
@Temperature 325 °F
Storage Temperature 20.0 - 100 °C68.0 - 212 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 102 - 113 °C215 - 235 °FMettler
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.0 - 2.01.0 - 2.0Molten
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 204 °C<= 400 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Coloroff-white
Suggested Application Temperature350°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL001 / 316792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.