MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP 525P PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP 525P is particularly developed for (biaxially) oriented PP film extrusion with a very specific molecular structure providing the ultimate properties required for the stretching process. Application:SABIC® PP 525P is typically used in mono layer or coextruded (B)OPP film. SABIC® PP 525P is known for its excellent metallisation behaviour. SABIC® PP 525P has a Food Contact Declaration. The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. This grade material is UL registered under File E111275. IMDS 7172624

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Antiblock Level 0.000 ppm
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPaSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Yield 10 %ISO 527-2 1A
Tensile Modulus 1550 MPaSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) 3.50 kJ/m²ISO 180/1A
Charpy Impact, Notched 4.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CFlat wise ( testbar 80*10*4mm); ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CFlat wise ( testbar 80*10*4mm); ISO 75
Vicat Softening Point 88.0 °Cat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 152 °Cat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentFalse
IsotacticityMedium
Molecular Weight DistributionBroad
Nucleating agentFalse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11198 / 244665

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.