Hostacom TRC 104N G13031 is a 20% talc filled PP copolymer, with good processability and high impact/stiffness balance. Product is available as a customized color matched, pellet form. This grade is delivered in G13031 color version. Applications: Instrument Panels, Interior TrimsInformation provided by LyondellBasell. |