MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 303 FR UV Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UV Stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. RTP 303 FR UV includes additional stabilization against UV degradation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D 792
Water Absorption 0.090 %
@Time 86400 sec
0.090 %
@Time 24.0 hour
ASTM D 570
Additive Loading 20 %20 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 103 MPa15000 psiASTM D 638
Elongation at Break 3.0 - 4.0 %3.0 - 4.0 %ASTM D 638
Tensile Modulus 6.21 GPa900 ksiASTM D 638
Flexural Strength 165 MPa24000 psiASTM D 790
Flexural Modulus 5.52 GPa800 ksiASTM D 790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.20 mm
2.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 6.94 J/cm
@Thickness 3.20 mm
13.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C290 °FASTM D 648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 5VB
@Thickness 3.00 mm
5VB
@Thickness 0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 266 - 316 °C510 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 305 FR UV Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UV Stabilized
Polykemi AB SCANTEC PC S75R GF20 Polycarbonate, Glass Fiber Reinforced
MRC Polymers NAXELL™ PC23M-20G General Purpose Low Viscosity Polycarbonate 20% Glass Fiber Reinforced
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
LNP Lubricomp® DFL-4032 BK8-250 Polycarbonate, Glass Fiber Reinforcement, PTFE Lubricant

PQZWA1152 / 90622

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.