MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot BLACK PEARLS® 630 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS® 630 specialty carbon black is a new product offering a balance of jetness and bluetone for use in a broad range of polymers for general purpose plastics applications. It is designed to offer additional color without sacrificing ease-of-dispersion characteristics of similar carbon blacks such as ELFTEX®570 carbon black (see Figure 1).

Key applications: BLACK PEARLS 630 specialty carbon black is suitable for use in general purpose moldings, such as for consumer goods, electronic materials and automotive parts. It is also suitable for use in polyester or polypropylene staple fibers, such as those used in carpets.

Performance features: BLACK PEARLS 630 specialty carbon black is designed to improve processability through higher loadings of carbon black in masterbatch and lower viscosity (as measured by MFI) without sacrificing color performance.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 325 Mesh325 Mesh<25 ppm; ASTM D-3265
 
Descriptive Properties
Iodine absorption136 mg/gASTM D-1510
OAN98 cc/100gASTM D-2414
Product FormPellets
Tint1.21ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT027 / 315762

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.