MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toyobo Pelprene™ P-280B Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: Key Feature: Pelprene P type

Pelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block copolymer consisting of an aromatic polyester as the hard segment and an aliphatic polyether as the soft one. It covers general purpose grades, being designed to have a balance of flexibility, heat & cold resistance, chemical resistance, and processability.

Information provided by Toyobo Co., Ltd

Key Words: Thermoplastic Elastomer; Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.30 %0.30 %25°C; 65%RH
Linear Mold Shrinkage 0.016 cm/cm
@Thickness 2.00 mm
0.016 in/in
@Thickness 0.0787 in
Melt Flow 13 g/10 min
@Temperature 230 °C
13 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9999ASTM D2240
Hardness, Shore D 6868ASTM D2240
Tensile Strength, Ultimate 21.0 MPa3050 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
50% Modulus 28.5 MPa
@Strain 50 %
28.5 MPa
@Strain 50 %
ASMT D638
Flexural Modulus 0.495 GPa71.8 ksiASTM D790
Compressive Modulus 0.0350 GPa5.08 ksi10% Compression Modulus; ASTM D695
Resilience 5555JIS K6301
Izod Impact, Notched 1.50 J/cm2.81 ft-lb/inASTM D256
Tear Strength 206 kN/m1180 pliASTM D624
Taber Abrasion, mg/1000 Cycles 8.08.0CS-17 wheel; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cmASTM D257
Dielectric Strength 30.0 kV/mm762 kV/inJIS K2111
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
77.8 µin/in-°F
@Temperature 68.0 °F
TMA
Melting Point 218 °C424 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FASTM D648
Vicat Softening Point 199 °C390 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FJIS K6301
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® TPU GF40 40% Glass Filled
Techmer ES HiFill® TPU GF30 30% Glass Filled
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer
Toyobo Pelprene™ P-30B Polyester TPE

PTOY36 / 70708

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.