MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAFLEX SG 45 HT A.01 black SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: TPE-S, Shore A46, black

Properties: flexible, good haptics, good recovery behavior, semi-crystalline, soft

Typical areas of application: Seals, Bellows, Haptic components, Toys

Industries: Automotive, Household appliances, Mechanical Engineering

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 46.046.0DIN ISO 7619-1
Tensile Strength at Break 3.30 MPa479 psiISO 527-1
Elongation at Break 250 %250 %ISO 527-1
Compression Set  0.400 %
@Treatment Temp. 23.0 °C
0.400 %
@Treatment Temp. 73.4 °F
ISO 815-1
 1.10 %
@Treatment Temp. 70.0 °C
1.10 %
@Treatment Temp. 158 °F
ISO 815-1
 1.90 %
@Treatment Temp. 100 °C
1.90 %
@Treatment Temp. 212 °F
ISO 815-1
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 240 °C392 - 464 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO557 / 326631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.