MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® A 225F Natural Nylon 66, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product Description: Ultramid® A 225F Natural is an unfilled polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles. This grade offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and excellent filling qualities. The UL94 V2 rating at 0.4mm makes that the product is particularly used in electrical applications.

Availability: Africa & Middle East; Latin America; North America

Features: Fast Molding Cycle; Good Dimensional Stability; Good Flow; Good Mold Release

Use: Consumer Applications; Electrical/Electronic Applications; Industrial Applications; Valves/Valve Parts; White Goods & Small appliances

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 1.1 %
@Time 86400 sec
1.1 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.3 MPa10200 psiISO 527-2
Tensile Strength, Yield 84.8 MPa12300 psiASTM D638
 95.1 MPa13800 psiISO 527-2/50
Elongation at Break 14 %14 %ASTM D638
 20 %20 %ISO 527-2
Elongation at Yield 5.0 %5.0 %ISO 527-2/50
Tensile Modulus 3.60 GPa522 ksiISO 527-1
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 3.15 GPa457 ksiISO 178
Izod Impact, Notched (ISO) 5.04 kJ/m²2.40 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 135 kJ/m²64.2 ft-lb/in²ASTM D256
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.399 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+15 ohm-cm4.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength  22.0 kV/mm
@Thickness 2.00 mm
560 kV/in
@Thickness 0.0787 in
IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
890 kV/in
@Thickness 0.0315 in
IEC 60243-1
Dissipation Factor 0.033
@Frequency 1e+6 Hz
0.033
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FUnannealed; ISO 75-2/A
Flammability, UL94  V-2
@Thickness 0.787 mm
V-2
@Thickness 0.0310 in
 V-2
@Thickness 3.30 mm
V-2
@Thickness 0.130 in
Glow Wire Flammability Index 699 °C
@Thickness 1.52 mm
1290 °F
@Thickness 0.0600 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 275 °C509 - 527 °F
Middle Barrel Temperature 270 - 280 °C518 - 536 °F
Front Barrel Temperature 280 - 285 °C536 - 545 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2080 / 310773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.