MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PVC-C®
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: PVC-C has high rigidity, strength, and hardness at increased temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %ISO 62
Water Absorption at Saturation 0.50 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ISO 868
Ball Indentation Hardness 150 MPaISO 2039
Tensile Strength at Break 80.0 MPaISO 527
 4910 psiASTM D638
Tensile Strength, Yield 49.0 MPaISO 527
 7090 psiASTM D638
Elongation at Break 15 %ISO 527
 23 %ASTM D638
Elongation at Yield 2.3 %ASTM D638
 5.0 %ISO 527
Modulus of Elasticity 2.57 GPaISO 527
 372 ksiASTM D638
Flexural Strength 76.0 MPaISO 178
 10600 psiASTM D638
Izod Impact, Notched 1.30 ft-lb/inASTM D256
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 27.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VKB; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 57.0 µin/in-°FASTM D696
 70.0 µm/m-°CISO 11359
Thermal Conductivity 0.140 W/m-K
@Temperature 20.0 °C
ISO 22007-4
Melting Point 110 °CDIN EN ISO 3146
Maximum Service Temperature, Air 85.0 °CUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75
 221 °FASTM D648
Vicat Softening Point 114 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -15.0 °CUL 746B
Glass Transition Temp, Tg 110 °CDIN EN ISO 3146
Flammability, UL94 V-0UL 94
Oxygen Index 65 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference; NSF-61 ,FDA
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
Chemical ResistanceDIN 8061
CKW Resistanceno
Colorlight grey
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistancelimited
Physiological indifferenceno, EEC
Resistance Against Hot Waterlimited
UV Stabilizationno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet
Overview of materials for Chlorinated PVC (CPVC)
Vycom Corzan® CPVC Chlorinated PVC
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding

PGEHR004 / 79841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.