MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Sika Builders’ Silicone Neutral cure, weather sealing building silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Sikasil Builders’ Silicone is a general purpose, moisture-cured, one-component, non-sag, elastomeric, neutral cure silicone sealant. for building applications. Meets the requirements of ASTM C-920, Type S, Grade NS, Class 25, use NT, T, M, G, A, O; TT-S-00230C, Type II, Class A; TT-S-001543A, Class A; CAN/ CGSB-19.13-M87, AAMA 802.3 Type II, AAMA 803.3, AAMA 805.2, AAMA 808.3 and California Air Resources Board 2003 requirements for Volatile Organic Compound content.

Where to Use:

  • As a weatherseal in conventional glazing
  • Window and door fabrication
  • Sealing expansion and control joints in precast concrete panels and metal curtain walls.
  • Perimeter sealing of doors, windows, skylights and other building components
  • Expansion and control joints
  • HVAC, white goods assembly
  • Glass, aluminum, tile, fiberglass, plastic, ceramic, masonry, concrete, brick and wood

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content 36 g/l36 g/l
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature -37.2 - 60.0 °C-35.0 - 140 °FApplication temp
Cure Time 20.0 min0.333 hourSkin Time (MNA method)
 1440 min24.0 hourASTM C679
Tack-Free Time 30.0 min0.500 hourASTM D679
Shelf Life 12.0 Month
@Temperature <=27.0 °C
12.0 Month
@Temperature <=80.6 °F
in original unopened cartridge
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sika Level Rapid Patch Fast-setting cementitious patch
Sika SikaFlex® 201 Adhesive
Sika SikaFlex 219 LM Low Modulus Polyurethane Sealant
Sika Level SkimCoat Fast setting, cement based smoothing and finishing compound
Sika AcouBond®-System Elastic Bonding and Acoustical Dampening

PSIKA902 / 209809

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.