MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior electrical insulation features are required. This smooth paste adhesive can be dispensed pneumatically, or by screen or pin transfer without stringing or tailing, and can position components before cure. TRA-BOND 2222 has a six month shelf life and develops strong, durable, solvent-resistant bonds - after a required high temperature cure cycle - to and between many different materials such as semiconductors, ceramics, glass, metals, and laminates. It is ideal for bonding chip-on-board, active and/or passive chip-type components in the fabrication of printed, integrated and hybrid circuits, and is just right for screen printing and epoxy die mounting applications, or for the assembly and repair of printed circuits, wave guides and electrical modules.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccMixed
Solids Content 100 %Reactive Solids Content
Volatile Organic Compounds (VOC) Content 2.29 g/l
Water Absorption 0.010 %After 24 hours
Viscosity 286000 cPMixed, degassed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Adhesive Bond Strength 730 psiLap shear, alum to alum, 15 min @ 100°C
 735 psiLap shear, alum to alum, 15 min @ 120°C
 1640 psiLap shear, alum to alum, 8 min @ 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+15 ohm-cm
Dielectric Constant 3.5
@Frequency 1000 Hz
Dielectric Strength 500 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg 75.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 min
@Temperature 150 °C
 15.0 min
@Temperature 120 °C
for higher property development
 >= 15.0 min
@Temperature 100 °C
Working Life 2160 hour
@Temperature 20.0 °C
 2160 hour
@Temperature 25.0 °C
 
Descriptive Properties
Color Red-Brown
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive
Lord Adhesives Thermoset™ MD-130 Electrically Insulating Die-Attach Adhesive

PTRAC065 / 70993

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.