MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Nuto 68 H Series
Categories: Fluid; Lubricant

Material Notes: Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high quality base oils and a select additive system that results in products that provide many desirable features to improve and prolong equipment life. Nuto H Series oils are designed to provide good performance in a range of hydraulic components used in systems subjected to moderate to severe operating conditions. Their high level oxidation and chemical stability helps control deposit formation and reduces the potential for sluggish system operation and valve sticking. They provide long oil/filter life and optimum equipment protection reducing both maintenance and product disposal costs. They provide good protection against rust and corrosion in high humidity operations or where low levels of moisture are unavoidable. Nuto H Series oils separate water readily and have good air release properties. These products meet the performance requirements of a wide range of hydraulic system and component OEMs.

Systems employing gear, vane, radial and axial piston pumps where anti-wear hydraulic oils are recommended; Hydraulic applications where contamination or leakage are unavoidable; Where small amounts of water are unavoidable and this water could damage components; Systems containing gears and bearings where mild anti-wear characteristics are required; Systems requiring load-carrying capability and anti-wear protection; Applications where thin oil-film corrosion protection is an asset such as systems where small amounts of water exist; Machines containing a wide range of components using various alloys in their designs

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.882 g/cc
@Temperature 15.0 °C
0.0319 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 107107Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 68 cSt68 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.5 cSt8.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -18.0 °C-0.400 °FASTM D97
Flash Point 234 °C453 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1A3 hrs @ 100°C
Demulsibility Time (min)20to 3 mL emulsion @ 54°C
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON087 / 75512

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.