MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Asahi Kasei TENAC™-C 850 Copolymer Acetal (POM), Electrically Conductive
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Excellent balance of mechanical properties, low friction and wear characteristics. Applications: Automotive parts, electrical & electronic parts, industrial parts.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm0.014 - 0.018 in/inAsahi Kasei
Melt Flow 15 g/10 min15 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50% RH; ISO 527
Elongation at Break 5.0 %5.0 %50% RH; ISO 527
Tensile Modulus 3.30 GPa479 ksi50% RH; ISO 527
Flexural Modulus 3.20 GPa464 ksi50% RH; ISO 178
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 - 100 ohm-cm10 - 100 ohm-cmIEC 60093
Surface Resistance 10 - 100 ohm10 - 100 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 153 °C307 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei TENAC™ 5010 Homopolymer Acetal (POM), Medium Viscosity
KEP Kepital® F20-03 Acetal Copolymer, Medium viscosity
Asahi Kasei TENAC™ 2010 Homopolymer Acetal (POM), High viscosity
Network Polymers Kepital® F20-03
Mitsubishi Iupital® F20-03 Copolymer Acetal

PASAHI8120 / 221147

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.