MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Titanvene™ LL0209SC LLDPE Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Titanvene™ LL0209SC is a linear low density polyethylene for high clarity film application. Titanvene™ LL0209SC is characterized by excellent transparency, low gel content, good process ability, and good mechanical properties with low blocking force and high slip.

Applications: Titanvene™ LL0209SC is typically used for: Shopping Bags; Food Packaging; Industrial Packaging; Rice Bag; Transparent Film; Garment Sack

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccISO 1183 Method D
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133 Condition 4
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.0 MPaSpeed I; ISO 1184(E)
Film Tensile Strength at Yield, TD 11.0 MPaSpeed I; ISO 1184(E)
Film Elongation at Break, MD 750 %Speed I; ISO 1184(E)
Film Elongation at Break, TD 800 %Speed I; ISO 1184(E)
Coefficient of Friction 0.140BS 2782, Method 824A
Dart Drop Test 130 gISO 7765-1 Method A
 
Thermal PropertiesOriginal ValueComments
Melting Point 122 °CISO 3146 Method C
Vicat Softening Point 103 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 14.0 %ASTM D1003
Gloss 50.0 %ASTM D2457
 
Descriptive Properties
Clarity (%)70ASTM D1746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOTT9607 / 326089

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.