MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin GFN3 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ GFN3 resin is a 30% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This general-purpose injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN3 carries a UL746C outdoor suitability rating of F2 and is an excellent candidate for a variety of indoor and outdoor applications including construction, electrical components + displays, lawn and garden equipment. *See NORYL GFN3F resin for FDA food compliant / NSF version.

Features: Hydrolytic Stability,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 300 °C
7.0 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 8.6 g/10 min
@Load 5.00 kg,
Temperature 300 °C
8.6 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 108108ASTM D785
Tensile Strength at Break 116 MPa16800 psi5 mm/min; ASTM D638
 117 MPa17000 psiISO 527
Elongation at Break 1.8 %1.8 %ISO 527
 2.0 %2.0 %5 mm/min; ASTM D638
Tensile Modulus 8.74 GPa1270 ksi1 mm/min; ISO 527
 9.15 GPa1330 ksi5 mm/min; ASTM D638
Flexural Strength 162 MPa23500 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 180 MPa26100 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 183 MPa26500 psiISO 178
Flexural Modulus 7.17 GPa1040 ksi2.6 mm/min, 100 mm span; ASTM D790
 8.00 GPa1160 ksi1.3 mm/min, 50 mm span; ASTM D790
 8.71 GPa1260 ksiISO 178
Izod Impact Notched 117 J86.3 ft-lbASTM D256
 124 J
@Temperature -30.0 °C
91.5 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.88 J/cm11.0 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²14.8 ft-lb/in²80*10*4; ISO 180/1U
 35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.90 J/cm²18.6 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 4.70 J/cm²
@Temperature -30.0 °C
22.4 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/2C
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/2C
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.93
@Frequency 50.0 - 60.0 Hz
2.93
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 21.6 kV/mm
@Thickness 3.20 mm
549 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  0.00 - 7.0 sec
@Thickness >=1.50 mm
0.00 - 7.0 sec
@Thickness >=0.0591 in
UL 746A
 7.0 - 15 sec
@Thickness >=3.00 mm
7.0 - 15 sec
@Thickness >=0.118 in
UL 746A
 60 - 120 sec
@Thickness >=6.00 mm
60 - 120 sec
@Thickness >=0.236 in
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
0.00 - 15 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 61.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 142 °C
@Thickness 3.20 mm
288 °F
@Thickness 0.126 in
unannealed; ASTM D648
 158 °C
@Thickness 6.40 mm
316 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 137 °C
@Thickness 3.20 mm
279 °F
@Thickness 0.126 in
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 143 °C289 °FRate B/50; ISO 306
 147 °C297 °FRate B/120; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82321 / 290268

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.