MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

ALM PA 601-CF Filled Nylon 12 Prototyping Polymer  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes:
  • Carbon fiber filled nylon 12 easy to process, strong light weight filled material.
  • Low density, good dimensional stability while maintaining excellent mechanical properties.
  • Fibers have been optimized to produce a smooth surface finish without sacrificing feature detail for tensile properties.
  • Excellent choice for rugged industrial applications with an HDT of ~177° C.

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.440 g/cc0.0159 lb/in³ASTM D1895
Density 1.07 g/cc0.0387 lb/in³Sintered; ASTM D792
Particle Size 50 µm50 µmD50
 35 - 100 µm35 - 100 µmD10-D90
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 235 °C
50 g/10 min
@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 66.0 MPa9570 psiXY; ASTM D638
Elongation at Break 3.6 %3.6 %XY; ASTM D638
Tensile Modulus 2.896 GPa420.0 ksiXY; ASTM D638
Flexural Modulus 3.447 GPa499.9 ksiXY; ASTM D790
Izod Impact, Notched 0.540 J/cm1.01 ft-lb/inASTM D256
Izod Impact, Unnotched 1.10 J/cm2.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.80e+14 ohm-cm7.80e+14 ohm-cm50% RH, 500V; ASTM D257
Surface Resistance 2.90e+14 ohm2.90e+14 ohm50% RH, 500V; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 184 °C363 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 178 °C352 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 177 °C351 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 16 LM PA12
Overview of materials for Nylon 6, Carbon Fiber Filled
Arkema Rilsamid® AECV BLACK 03 TL PA12
Arkema Rilsamid® AMN BLACK P40 TLD PA12
Overview of materials for Nylon 12

PALP81 / 177142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.