MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huafon JF-P-509/JF-I-609T Polyether
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Characteristics: Polyether resin of medium to high hardness, excellent temperature and hydrolysis resistance.

Applications: For man/woman shoes and casual shoes.

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.300 - 0.350 g/cc0.0108 - 0.0126 lb/in³Free rise foam density
 0.600 - 0.700 g/cc0.0217 - 0.0253 lb/in³Product
 1.00 - 1.02 g/cc
@Temperature 40.0 °C
0.0361 - 0.0368 lb/in³
@Temperature 104 °F
JF-P-509
 1.12 - 1.14 g/cc
@Temperature 40.0 °C
0.0405 - 0.0412 lb/in³
@Temperature 104 °F
JF-I-609T
Viscosity  200 - 600 cP
@Temperature 40.0 °C
200 - 600 cP
@Temperature 104 °F
JF-I-609T
 400 - 700 cP
@Temperature 40.0 °C
400 - 700 cP
@Temperature 104 °F
JF-P-509
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 3.50 MPa>= 508 psi
Elongation at Break >= 350 %>= 350 %
Tear Strength >= 20.0 kN/m>= 114 pli
Abrasion >= 15>= 15
 
Processing PropertiesMetricEnglishComments
Mold Temperature 45.0 - 55.0 °C113 - 131 °F
 
Descriptive Properties
AppearanceLiquid or waxy40°C, JF-P-509
 Transparent and pure liquid40°C, JF-I-609T
Asker A Hardness60-65
Asker C Hardness70-75
Cream time5-8 sec
Demold time4-6 min
Depression of physical properties<20%after two weeks hydrolysis test
Flexing resistanceNo crack-40°C, Breakage length, outsole
Material Temperature33-37°C
 38-42°C
P+C/l Mix ratio100/84-86
Rise time25-35 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUAF036 / 294979

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.