MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® K 3433 Polymer-based Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® K 3433 is a weakly basic, macroporous, palladium-doped, polymer-based resin in spherical bead form. It is designed to catalytically remove dissolved oxygen from water. A suitable reducing agent such as hydrogen is dissolved in the water to be treated and then passed through a bed of the catalyst. By this method, residual oxygen concentrations of less than 20 ppb can be obtained at flow rates up to 80 m/h and temperatures up to 120°C. Lewatit K 3433 is designed for the following applications:
  • Removal of dissolved oxygen from water for drinks production
  • Removal of dissolved oxygen from sea water used in offshore oilfield injection
  • For oxygen removal for boiler feed water and heating circuits.

    Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.670 g/cc
Density 1.02 g/cc
Bead Size 0.400 - 1.25 mm>90%
Storage Temperature -20.0 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceGray, opaque
pH Operating Range5 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PLANY8761 / 209153

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.