MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dioshy HP-907NC SEBS Series
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Features:
  • Silicone and rubber touch; broad hardness range (Shore A 0 ~ Shore D65).
  • Passed US FDA and EU LFGB food application standards, medical grades are also included.
  • Excellent anti-slip and good tensile strength; transparent or white color, good coloring ability; customized.
  • Suitable to dual color processing for PP or PE; also can be the toughener for PP or PE.
  • Suitable to mostly thermoplastic procedures; PVC replacement.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC .

Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.871 g/cc0.871 g/ccJIS-K6301
Melt Flow 12.84 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12.84 g/10 min
@Load 4.76 lb,
Temperature 374 °F
JIS-K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7.07.0JIS-K6301
Tensile Strength 1.96 MPa284 psiJIS-K6310
Elongation at Break 839 %839 %JIS-K6310
100% Modulus 0.0981 MPa14.2 psiJIS-K6310
300% Modulus 0.0981 MPa14.2 psiJIS-K6310
Tear Strength 108 kN/m616 pliJIS-K6310-B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 140 - 160 °C284 - 320 °FInjection
Middle Barrel Temperature 170 - 180 °C338 - 356 °FInjection
Front Barrel Temperature 175 - 185 °C347 - 365 °FInjection
Nozzle Temperature 185 - 195 °C365 - 383 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIOSH018 / 294628

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.