MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin PKN4752F Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4752F resin is a non-reinforced, translucent, high heat blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrudable and injection moldable grade is FDA food contact compliant and exhibits high heat resistance, dimensional stability, and appears translucent with a yellow tint in the natural color. NORYL PKN4752F resin is an excellent candidate for high performance packaging in food, electronics, and healthcare. *See NORYL PKN4752 resin for NON FDA compliant version.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Low Warpage,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Moisture Absorption 0.000 %0.000 %Sheet Extrusion
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 73.0 MPa10600 psi50 mm/min; ASTM D638
Tensile Strength, Yield 86.0 MPa12500 psi50 mm/min; ASTM D638
Elongation at Break 15 %15 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
Tensile Modulus 3.00 GPa435 ksi50 mm/min; ASTM D638
Flexural Strength 136 MPa19700 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 144 MPa20900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.94 GPa426 ksi2.6 mm/min, 100 mm span; ASTM D790
 3.15 GPa457 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 32.0 J23.6 ft-lbASTM D256
Dart Drop, Total Energy 6.00 J4.43 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 55.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
31.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 3.20 mm
320 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  151 °C
@Thickness 3.20 mm
304 °F
@Thickness 0.126 in
unannealed; ASTM D648
 151 °C
@Thickness 6.40 mm
304 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 173 °C343 °FRate B/50; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 205 - 225 °C401 - 437 °FSheet Extrusion
Zone 2 215 - 240 °C419 - 464 °FSheet Extrusion
Zone 3 240 - 265 °C464 - 509 °FSheet Extrusion
Zone 4 240 - 265 °C464 - 509 °FSheet Extrusion
Adapter Temperature 240 - 265 °C464 - 509 °FSheet Extrusion
Die Temperature 240 - 265 °C464 - 509 °FSheet Extrusion
Melt Temperature 265 - 275 °C509 - 527 °FSheet Extrusion
Roll Temperature 105 - 120 °C221 - 248 °FRoll Stack Temp - Bottom
 105 - 120 °C221 - 248 °FRoll Stack Temp - Middle
 105 - 120 °C221 - 248 °FRoll Stack Temp - Top
Drying Temperature 70.0 - 80.0 °C158 - 176 °FSheet Extrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourSheet Extrusion
 8.00 hour8.00 hourCumulative; Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82417 / 290364

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.