MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Master Bond LED401 White One Component LED Curable Adhesive System
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In fact, this unique system will fully cure tack-free without any oxygen inhibition. This technology allows LED401 White to be utilized not only as an adhesive, but as a sealant, coating and encapsulation system. This system can cure in sections up to and beyond 1/8 inch thick upon exposure to the LED light. Since it is a LED curable system, it is intrinsically safer than one requiring UV light for polymerization, as LED light emitting sources are generally considered to be safer and more user friendly than their comparable UV counterparts. Master Bond LED401 White requires no mixing and will cure rapidly, with the speed of cure dependent upon the intensity of the light source, the thickness of the layer and the distance of the light source from the material being cured. Realistically, the light intensity should be 1-4 watts/cm2. Master Bond strongly advises end users to consult with their light source provider to ascertain the best LED for their particular application, along with details on the wavelength being emitted by the light source. In thinner sections, full cures can be achieved in 15-30 seconds (sometimes less than that), while thicker sections require longer cure times. Once cured, LED401 White has excellent dimensional stability, good electrical insulation properties and very good chemical resistance to water, many acids, bases and oils. It also bonds well to glass, polycarbonates and acrylics, along with other plastics and metals. Prior to cure, it has a high viscosity consistency, but it remains flowable. Additionally, the formulation is solvent-free. This product is opaque white color which adds a special dimension to light initiated curing systems, since nearly all are either transparent or tinted with dyes.

Product Advantages:

  • Requires LED light source emitting light at 405 nm wavelength; no UV light required.
  • One component system; no mixing needed; ready to use as supplied.
  • Fast curing upon exposure to appropriate light source.
  • No oxygen inhibition while curing; will fully cure beyond 1/8 inch.
  • White color, totally opaque.
  • Very good dimensional stability.
  • Exceptional physical properties.
  • High bond strength with superior adhesion to surface treated metals, glass and many plastics.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity >= 350000 cP>= 350000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 7065 - 70
Tensile Strength at Break >= 24.1 MPa>= 3500 psi
Tensile Modulus >= 1.38 GPa>= 200 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.9
@Frequency 60 Hz,
Temperature 25.0 °C
3.9
@Frequency 60 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 65.0 µm/m-°C33.3 - 36.1 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 70.0 - 75.0 °C158 - 167 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Monthin original unopened container s, with no exposure to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond LED405Med One component, nanosilica filled LED curable system
Cookson Group Plaskon® SMT-B-2FPI Molding Compound for PBGA and CSP
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating

PMASTB415 / 149662

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.