MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ho Hsiang Ching HA-700W SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The HA series belongs to the SEBS (STYRENE-ETHYLENE/BUTYLENE- STYRENE) hydrogenated and alloyed grade of materials. The materials of the HA series are slip resistant, soft and comfortable, look good and has excellent mechanical strength and scratch resistance. It can be combined with ABS and PC materials with excellent shot sticky strength. When used in high precision steel mold production, no matter what the finished product is accessory or small part, its products are able to reach an excellent level of consistency and function. For example, the thermoplastic elastomer material (TPE/TPS) in coating on 3C product and medical product is a good choice with regards to both performance and value. HHC's HA series can meet the needs of such commercialization, and it is the best choice for customers' needs! Suitable for most of the thermoplastic processing methods, such as injection molding, extrusion molding and so on. This material complies with EU RoHS, REACH-SVHC regulations and has passed the Nylon Phenol Ethoxylates (NPEO), Polynuclear aromatic hydrocarbons (PAHs) and phthalates (6P, Nylonphenol) and other safety tests. It is a non-toxic and safe material with environmentally friendly specifications.

Color: Natural Color / Black Color / Customized Color

The optimum combination of materials: ABS, PC

Processing: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Applications: Sport goods, pneumatic tools, power tools, etc.

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength 5.79 MPa839 psiASTM 412C
Elongation at Break 575 %575 %ASTM 412C
Tear Strength 26.5 kN/m151 pliASTM 412C
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 100 °C212 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 351 °F
Middle Barrel Temperature 166 - 182 °C331 - 360 °F
Front Barrel Temperature 177 - 191 °C351 - 376 °F
Nozzle Temperature 182 - 204 °C360 - 399 °F
Mold Temperature 16.0 - 66.0 °C60.8 - 151 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Hold Pressure 14.0 - 48.0 MPa2030 - 6960 psi
Back Pressure 0.340 - 0.690 MPa49.3 - 100 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHSIANG049 / 312525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.